Pages 262-268, Language: EnglishInoue / Murakami / TeradaNickel-chromium alloys were plated with tin and chromium to evaluate the effect on porcelain shear bond strength. Six plating methods were used. Additionally, the microstructure of the bond between the plated alloy and porcelain were studied using SEM and EPMA. Tin plating increased the bond strength of porcelain to a nickel-chromium alloy while chromium plating did not.